How do I stop press brake tooling marking the part?

Marks come from contact pressure at the punch tip and the die shoulders. The practical fixes are a urethane die, a wider die opening, a protective film at the contact points, and a polished or coated tool.

What causes marks on a bent part?

Two mechanisms: the sliding contact at the punch tip as the material bends, and the pressure against the die shoulder. Softer and coated materials show both more readily.

Mark types and their cause
MarkCauseTypical fix
Line across the inside at the tipPunch tip contact pressureLarger tip radius, film, polish
Line on the outside at the die shoulderShoulder pressureWider die opening, urethane, film
Scuffing along the bendSliding contact and gallingLubrication, coated tool, polished surface
Indentation at a pointDebris or a damaged toolClean and inspect the tooling

What is anti-mark tooling?

Anti-mark tooling reduces or moves the contact pressure so the visible face is not marked. It includes urethane dies, dies with radiused or reduced shoulders, punch tips with a larger radius, and tools with a protective coating.

  • Urethane die: the insert carries the contact, so steel never touches the face.
  • Radiused shoulders: spread the pressure over a wider area.
  • Larger punch tip radius: reduces tip pressure but increases the bend radius.
  • Protective film or insert: a consumable that takes the contact instead of the part.
  • Coated tool: reduces friction and galling, which limits scuffing.

When is a protective film better than a urethane die?

A film is better when the drawing specifies a tight radius, because it does not change the radius. A urethane die changes the radius to a larger, load-dependent value, which may not suit the part.

Film is a consumable and has to be replaced, and it can itself leave a faint line if it creases. For a repeat job, a coating or a radiused die is usually the more durable answer.

Does lubricating the material help?

It reduces sliding friction, which limits scuffing and galling, but it does not remove the pressure marks at the contact points. It also has to be cleaned off afterwards, which matters for painted parts.

For pre-painted or coated sheet, check that any lubricant used is compatible with the coating before running production.

Related technical pages

Urethane dies

Mar-free forming with an elastomer insert.

Radius dies

Radiused shoulders that spread the contact pressure.

Press brake dies

Die types and openings, and how the opening affects marking.

Troubleshooting

Diagnosing marks and the other common faults.

Next step

Send a sample of the material and a photograph of the mark and we will recommend the tooling or surface treatment that removes it.

Request a quotation

Send an enquiry

Tell us the machine make and model, or describe the tooling you need. We reply to every enquiry within one business day, and quote from a drawing for special profiles.

Prefer email? Write to [email protected] — enquiries from this form go to the same address.